About the article
D.A. BARCHUKOV
The results of studies of the microstructure, microhardness, microgeometry of the laser cut surface of deposited high-speed steel grade R9M4K8 after diamond burnishing are presented. It has been shown that the surface roughness of a laser cut is reduced by 3...4 times, which makes it possible to obtain a working surface without subsequent mechanical grinding. It is noted that diamond smoothing leads to microstructure refinement, increase of steel microhardness up to 9 700 ± 130 MPa.
laser cutting, steel, diamond burnishing, roughness, microstructure, microhardness.